This was an ornament I printed roughly 6 years ago. Being a Christmas ornament it spent most of those 6 years stored in my roof space.

Being in Australia this would have been subject to average temperatures of 30 to 35 degrees c but also peaks across summer approaching 70 degrees c. Also in high humidity.

The PLA crumbles into tiny pieces at the softest touch.

I thought it was interesting that PLA would start to break down in these conditions.

  • Cyrus Draegur@lemm.ee
    link
    fedilink
    English
    arrow-up
    5
    arrow-down
    6
    ·
    4 days ago

    it’s a starch-based polymer, isn’t it? it will be readily metabolized by the various ubiquitous species populating our biosphere. i suppose it’s a good thing. possibly the only microplastic that doesn’t suck